PRICES include / exclude VAT
immediate downloadReleased: 2024-05-16
24/30463784 DC
BS ISO 18177 Plastics - Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC)
Format
Availability
Price and currency
English Secure PDF
Immediate download
23.00 EUR
English Hardcopy
In stock
23.00 EUR
Standard number: | 24/30463784 DC |
Pages: | 29 |
Released: | 2024-05-16 |
Status: | Draft for Comment |
DESCRIPTION
24/30463784 DC
This standard 24/30463784 DC BS ISO 18177 Plastics - Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC) is classified in these ICS categories:
- 83.080.20 Thermoplastic materials