PRICES include / exclude VAT
Homepage>ASTM Standards>ASTM A1032-15R19 - Standard Test Method for Hydrogen Embrittlement Resistance for Steel Wire Hard-Drawn Used for Prestressed Concrete Pipe
Sponsored link
Released: 01.11.2019

ASTM A1032-15R19 - Standard Test Method for Hydrogen Embrittlement Resistance for Steel Wire Hard-Drawn Used for Prestressed Concrete Pipe

Standard Test Method for Hydrogen Embrittlement Resistance for Steel Wire Hard-Drawn Used for Prestressed Concrete Pipe

Format
Availability
Price and currency
English PDF
Immediate download
52.97 EUR
English Hardcopy
In stock
52.97 EUR
Standard number:ASTM A1032-15R19
Released:01.11.2019
Status:Active
Pages:3
Section:01.04
Keywords:cracking; hard-drawn steel wire; hydrogen embrittlement; prestressed concrete pipe; prestressing;
DESCRIPTION

1.1 This test method describes procedures to determine the hydrogen embrittlement (HE) resistance of hard-drawn steel wire used for prestressed concrete pipe.

1.2 HE resistance is reported as time-to-failure of specimens tested in a laboratory.

1.3 The values stated in SI units are to be regarded as standard. The values given in parentheses after SI units are provided for information only and are not considered standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.