PRICES include / exclude VAT
Homepage>ASTM Standards>91>91.100>91.100.50>ASTM D7906-22 - Standard Practice for Recovery of Asphalt Binder from Solution Using Toluene and the Rotary Evaporator
Sponsored link
Released: 01.05.2022

ASTM D7906-22 - Standard Practice for Recovery of Asphalt Binder from Solution Using Toluene and the Rotary Evaporator

Standard Practice for Recovery of Asphalt Binder from Solution Using Toluene and the Rotary Evaporator

Format
Availability
Price and currency
English PDF Redline
Immediate download
63.56 EUR
English PDF
Immediate download
52.97 EUR
English Hardcopy
In stock
52.97 EUR
Standard number:ASTM D7906-22
Released:01.05.2022
Status:Active
Pages:4
Section:04.03
Keywords:bituminous paving mixtures; RAP; RAS; recovery; recycled asphalt pavement; recycled asphalt shingles; rotary evaporator;
DESCRIPTION

1.1 This practice is intended to be used to recover asphalt from a solvent using the rotary evaporator to ensure that changes in the asphalt properties during the recovery process are minimized.

1.2 Units—The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.