PRICES include / exclude VAT
Homepage>ASTM Standards>25>25.220>25.220.99>ASTM F2024-10R21 - Standard Practice for X-ray Diffraction Determination of Phase Content of Plasma-Sprayed Hydroxyapatite Coatings
Sponsored link
Released: 01.02.2021

ASTM F2024-10R21 - Standard Practice for X-ray Diffraction Determination of Phase Content of Plasma-Sprayed Hydroxyapatite Coatings

Standard Practice for X-ray Diffraction Determination of Phase Content of Plasma-Sprayed Hydroxyapatite Coatings

Format
Availability
Price and currency
English PDF
Immediate download
52.97 EUR
English Hardcopy
In stock
52.97 EUR
Standard number:ASTM F2024-10R21
Released:01.02.2021
Status:Active
Pages:4
Section:13.01
Keywords:amorphous calcium phosphate (ACP); hydroxyapatite coatings; hydroxyapatite (HAP); hydroxylapatite coatings; phase analysis; tricalcium phosphate; whitlockite;
DESCRIPTION

1.1 This practice is for the determination, by the Reference Intensity Ratio External Standard Method, of the percent by weight of the crystalline phases, hydroxyapatite (HA), beta-(whitlockite) tricalcium phosphate (β-TCP), and calcium oxide (CaO) in coatings deposited upon metallic substrates by plasma spraying hydroxyapatite.

1.2 A major component in plasma-sprayed HA coatings other than HA is expected to be amorphous calcium phosphate (ACP). Crystalline components other than HA that may be present include alpha- and beta- (whitlockite) tricalcium phosphates, tetracalcium phosphate (TTCP), calcium oxide, and calcium pyrophosphates. Quantification of the minor crystalline components has proven to be very unreliable due to extreme overlap and confounding of X-ray diffraction peaks. Therefore, this practice addresses the quantification of only HA, β-TCP, and CaO.

1.3 This practice was developed for plasma-sprayed HA coatings with HA contents of at least 50 % of the total coating. It is recognized that the analysis of the crystalline components uses diffraction from regions of the pattern that also include a small contribution from the amorphous component. However, within the limits of applicability of this practice, the effect of such interference is believed to be negligible.

1.4 The coating analyzed shall be produced and processed under manufacturing conditions equivalent to those used on the device of interest.

1.5 This practice requires the use of monochromated copper Kα radiation and flat samples.

1.6 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.7 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.8 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.