PRICES include / exclude VAT
Sponsored link
immediate downloadReleased: 2010-01-31
BS 2HR 6:2010
Specification for nickel-chromium- iron-molybdenum-cobalt-tungsten heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 21.7, Fe 18.5, Mo 9, Co 1.5, W 0.6)
Format
Availability
Price and currency
English Secure PDF
Immediate download
151.20 EUR
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standardfor 1 hour
15.12 EUR
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standardfor 24 hours
45.36 EUR
English Hardcopy
In stock
151.20 EUR
Standard number: | BS 2HR 6:2010 |
Pages: | 14 |
Released: | 2010-01-31 |
ISBN: | 978 0 580 67044 2 |
Status: | Standard |
DESCRIPTION
BS 2HR 6:2010
This standard BS 2HR 6:2010 Specification for nickel-chromium- iron-molybdenum-cobalt-tungsten heat-resisting alloy billets, bars, forgings and parts (nickel base, Cr 21.7, Fe 18.5, Mo 9, Co 1.5, W 0.6) is classified in these ICS categories:
- 49.025.99 Other materials
This British Standard specifies requirements for nickel-chromiumiron-molybdenum-cobalt-tungsten heat-resisting alloy supplied in the following forms, and as parts.
Bars and extruded sections for machining: annealed, designation HR 6A.
Billets and bars for forging: hot or cold worked and subsequently machined or ground, designation HR 6B.
Forgings: annealed, designation HR 6C.