PRICES include / exclude VAT
Homepage>BS Standards>55 PACKAGING AND DISTRIBUTION OF GOODS>55.120 Cans. Tins. Tubes>BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test
Sponsored link
immediate downloadReleased: 2017-02-28
BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test

BS EN 15384-2:2017

Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test

Format
Availability
Price and currency
English Secure PDF
Immediate download
162.14 EUR
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
16.21 EUR
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
48.64 EUR
English Hardcopy
In stock
162.14 EUR
Standard number:BS EN 15384-2:2017
Pages:12
Released:2017-02-28
ISBN:978 0 580 91014 2
Status:Standard
DESCRIPTION

BS EN 15384-2:2017


This standard BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes is classified in these ICS categories:
  • 55.120 Cans. Tins. Tubes

This European Standard is applicable for internally coated cylindrical aluminium tubes, mainly used for the packing of pharmaceutical, cosmetic, hygiene, food or other household products.

The internal coating is used as a barrier and should avoid any contact between aluminium and the product. This standard defines the copper sulphate method to detect the electrolyte conductivity as one criterion for the quality of the internal coating.

The electrolyte conductivity of the internal coating is only one criterion for evaluation of the quality of an internal coating. It does not give any information on the quantity or size of any pores or uncoated areas, nor any hint on possible reactions between the aluminium tube and the product. The electrolyte conductivity should never be used as the sole criterion for quality evaluation of the internal coating, but always with other parameters e.g. film thickness, acetone and/or ammonia resistance and of course results of enhanced stability studies.