BS EN 4826:2014
Aerospace series. Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength ≤ 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners
Standard number: | BS EN 4826:2014 |
Pages: | 18 |
Released: | 2014-12-31 |
ISBN: | 978 0 580 86330 1 |
Status: | Standard |
BS EN 4826:2014
This standard BS EN 4826:2014 Aerospace series. Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength ≤ 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners is classified in these ICS categories:
- 49.040 Coatings and related processes used in aerospace industry
This European Standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels ( R m ≤ 1 450 MPa), stainless steels ( R m ≤ 1 450 MPa), copper alloys, nickel alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard.
The purpose of this standard is to give technical and quality requirements of Zinc-Nickel plating. It doesn’t give complete in-house process instructions, these shall be given in the manufacturers detailed process instructions.