BS EN ISO 11357-5:2014 Plastics. Differential scanning calorimetry (DSC) Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

BS EN ISO 11357-5:2014

Plastics. Differential scanning calorimetry (DSC) Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion

Format
Availability
Price and currency
English Secure PDF
Immediate download
181.70 EUR
English Hardcopy
In stock
181.70 EUR
Standard number:BS EN ISO 11357-5:2014
Pages:20
Released:2014-04-30
ISBN:978 0 580 83435 6
Status:Standard
DESCRIPTION

BS EN ISO 11357-5:2014


This standard BS EN ISO 11357-5:2014 Plastics. Differential scanning calorimetry (DSC) is classified in these ICS categories:
  • 83.080.01 Plastics in general

This part of ISO 11357 specifies a method for the determination of reaction temperatures and times, enthalpies of reaction, and degrees of conversion using differential scanning calorimetry (DSC).

The method applies to monomers, prepolymers, and polymers in the solid or liquid state. The material can contain fillers and/or initiators in the solid or liquid state.