BS ISO 18373-1:2007 Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the processing temperature

BS ISO 18373-1:2007

Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the processing temperature

Format
Availability
Price and currency
English Secure PDF
Immediate download
181.70 EUR
English Hardcopy
In stock
181.70 EUR
Standard number:BS ISO 18373-1:2007
Pages:18
Released:2007-09-28
ISBN:978 0 580 56391 1
Status:Standard
DESCRIPTION

BS ISO 18373-1:2007


This standard BS ISO 18373-1:2007 Rigid PVC pipes. Differential scanning calorimetry (DSC) method is classified in these ICS categories:
  • 23.040.20 Plastics pipes

This part of ISO 18373 specifies a method for the determination of the processing temperature of rigid PVC pipe samples. The method is based on the measurement of the thermal history using differential scanning calorimetry (DSC) and is suitable for all types of rigid PVC pipes.