PRICES include / exclude VAT
Homepage>CSN Standards>31 AERONAUTICS AND COSMONAUTICS>3182 Surface protection and preparation, incl. hardening>CSN EN 4826 - Aerospace series - Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength <= 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners
Sponsored link
Released: 01.07.2015
CSN EN 4826 - Aerospace series - Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength <= 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners

CSN EN 4826

Aerospace series - Zinc-Nickel (12 %-16 % Ni) plating of steels with specified tensile strength <= 1 450 MPa, copper alloys, nickel alloys and aluminium alloys for parts and fasteners

Format
Availability
Price and currency
English Hardcopy
In stock
52.00 EUR
FREE Shipping
Number of Standard:CSN EN 4826
Category:318216
Pages:20
Released:01.07.2015
Catalog number:97270
DESCRIPTION

CSN EN 4826

CSN EN 4826 This European Standard specifies the plating of a Zinc-Nickel (12 % to 16 %) alloy on mechanical parts and fasteners in steels (Rm <= 1 450 MPa), stainless steels (Rm <= 1 450 MPa), copper alloys, nickel alloys and aluminium alloys (not applicable for electrical components), as well as the passivation and lubricant finishing that can be associated to them. The Zinc-Nickel process is an electrolytic plating process under controlled current allowing to deposit a Zinc-Nickel layer from, most often, an alkaline electrolyte. Alkaline Zinc-Nickel is only considered in this standard. The purpose of this standard is to give technical and quality requirements of Zinc-Nickel plating. It doesn't give complete in-house process instructions, these shall be given in the manufacturers detailed process instructions.
Original English text of CSN EN Standard.
The price of the Standard included all amendments and correcturs.