Don't have a credit card? Never mind we support BANK TRANSFER .

PRICES include / exclude VAT
Homepage>CSN Standards>64 PLASTICS>6407 Testing of plastics and plastic products>CSN EN ISO 11357-4 - Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity
Released: 01.09.2021
CSN EN ISO 11357-4 - Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity

CSN EN ISO 11357-4

Plastics - Differential scanning calorimetry (DSC) - Part 4: Determination of specific heat capacity

Format
Availability
Price and currency
English Hardcopy
In stock
61.00 EUR
FREE Shipping
Number of Standard:CSN EN ISO 11357-4
Category:640748
Pages:24
Released:01.09.2021
Catalog number:512591
DESCRIPTION

CSN EN ISO 11357-4

CSN EN ISO 11357-4 This document specifies methods for determining the specific heat capacity of plastics by differential scanning calorimetry.
Original English text of CSN EN Standard.
The price of the Standard included all amendments and correcturs.