Homepage>DIN Standards>DIN EN ISO 11357-5 Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion (ISO 11357-5:2013)
in stockReleased: 2014-07
DIN EN ISO 11357-5 Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion (ISO 11357-5:2013)

DIN EN ISO 11357-5

Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion (ISO 11357-5:2013)

Kunststoffe - Dynamische Differenz-Thermoanalyse (DSC) - Teil 5: Bestimmung von charakteristischen Reaktionstemperaturen und -zeiten, Reaktionsenthalpie und Umsatz (ISO 11357-5:2013)

Format
Availability
Price and currency
English PDF
Immediate download
99.44 EUR
English Hardcopy
In stock
99.44 EUR
German PDF
Immediate download
79.73 EUR
German Hardcopy
In stock
79.73 EUR
Status:Standard
Released:2014-07
Standard number:DIN EN ISO 11357-5
Name:Plastics - Differential scanning calorimetry (DSC) - Part 5: Determination of characteristic reaction-curve temperatures and times, enthalpy of reaction and degree of conversion (ISO 11357-5:2013)