Main page>DIN Standards>DIN EN ISO 7539-6 Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement (ISO 7539-6:2018, Corrected version 2018-11 + Amd 1:2024) (includes Amendment A1:2024)
in stockReleased: 2024-09
DIN EN ISO 7539-6 Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement (ISO 7539-6:2018, Corrected version 2018-11 + Amd 1:2024) (includes Amendment A1:2024)

DIN EN ISO 7539-6

Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement (ISO 7539-6:2018, Corrected version 2018-11 + Amd 1:2024) (includes Amendment A1:2024)

Korrosion der Metalle und Legierungen - Prüfung der Spannungsrisskorrosion - Teil 6: Vorbereitung und Anwendung von angerissenen Proben für die Prüfung unter konstanter Last oder konstanter Auslegung (ISO 7539-6:2018, korrigierte Fassung 2018-11 + Amd 1:2024) (enthält Änderung A1:2024)

Format
Availability
Price and currency
English PDF
Immediate download
Printable
190.49 EUR
English Hardcopy
In stock
190.49 EUR
German PDF
Immediate download
Printable
152.14 EUR
German Hardcopy
In stock
152.14 EUR
Status:Standard
Released:2024-09
Standard number:DIN EN ISO 7539-6
Name:Corrosion of metals and alloys - Stress corrosion testing - Part 6: Preparation and use of precracked specimens for tests under constant load or constant displacement (ISO 7539-6:2018, Corrected version 2018-11 + Amd 1:2024) (includes Amendment A1:2024)
Pages:50
DESCRIPTION

DIN EN ISO 7539-6