Don't have a credit card? Never mind we support BANK TRANSFER .

PRICES include / exclude VAT
Homepage>IEC Standards>IEC TR 62036:2007 - Mineral insulating oils - Oxidation stability test method based on differential scanning calorimetry (DSC)
download between 0-24 hoursReleased: 2007-04-11
IEC TR 62036:2007 - Mineral insulating oils - Oxidation stability test method based on differential scanning calorimetry (DSC)

IEC TR 62036:2007

Mineral insulating oils - Oxidation stability test method based on differential scanning calorimetry (DSC)

Huiles minérales isolantes - Méthode d'essai pour évaluer la stabilité d'oxydation fondée sur l'analyse calorimétrique différentielle par balayage

Format
Availability
Price and currency
English/French - Bilingual PDF
Immediate download
88.00 EUR
English/French - Bilingual Hardcopy
in stock
88.00 EUR
Standard number:IEC TR 62036:2007
Released:2007-04-11
Language:English/French - Bilingual
DESCRIPTION

IEC TR 62036:2007

To develop a rapid oxidation stability test method based on differential scanning calorimetry (DSC) to assess the oxidation stability of mineral insulating oils