Homepage>ISO Standards>ISO 11409:1993-Plastics — Phenolic resins — Determination of heats and temperatures of reaction by differential scanning calorimetry
download between 0-24 hoursReleased: 1993
ISO 11409:1993-Plastics — Phenolic resins — Determination of heats and temperatures of reaction by differential scanning calorimetry

ISO 11409:1993

ISO 11409:1993-Plastics — Phenolic resins — Determination of heats and temperatures of reaction by differential scanning calorimetry

Format
Availability
Price and currency
English PDF
Immediate download
77.78 USD
English Hardcopy
In stock
77.78 USD
French PDF
Immediate download
77.78 USD
French Hardcopy
In stock
77.78 USD
Standard´s number:ISO 11409:1993
Pages:7
Edition:1
Released:1993
DESCRIPTION

ISO 11409:1993


The principle of the method specified is measuring the heat flux supplied to a test sample as a function of time or temperature, while the test sample is subjected to a temperature schedule under a specified atmosphere. A reaction is marked by the release of energy from the sample, resulting in an exothermic peak in the heating curve. Integration of the recorded peak area as a function of time gives a measure of the energy of the reaction. Applies to phenolic resins with exothermic behaviour, such as resols or mixtures of novolaks with hexamethylenetetramine or other curing agents.