ISO 11463:2020-Corrosion of metals and alloys — Guidelines for the evaluation of pitting corrosion

ISO 11463:2020

ISO 11463:2020-Corrosion of metals and alloys — Guidelines for the evaluation of pitting corrosion

Format
Availability
Price and currency
English PDF
Immediate download
115.00 EUR
English Hardcopy
In stock
115.00 EUR
French PDF
Immediate download
115.00 EUR
French Hardcopy
In stock
115.00 EUR
Standard´s number:ISO 11463:2020
Pages:12
Edition:2
Released:2020
DESCRIPTION

ISO 11463:2020


This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.