ISO 14322:2018-Plastics — Epoxy resins — Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

ISO 14322:2018

ISO 14322:2018-Plastics — Epoxy resins — Determination of degree of crosslinking of crosslinked epoxy resins by differential scanning calorimetry (DSC)

Format
Availability
Price and currency
English PDF
Immediate download
70.00 EUR
English Hardcopy
In stock
70.00 EUR
Standard´s number:ISO 14322:2018
Pages:8
Edition:2
Released:2018
Language:English
DESCRIPTION

ISO 14322:2018


This document specifies a method whereby the heat of reaction generated during epoxy resin crosslinking is measured by differential scanning calorimetry (DSC). The degree of crosslinking is determined based on this result. This method is applicable to epoxy resin systems with a moderate or slow crosslinking-reaction speed. It might not be applicable to systems with a fast crosslinking-reaction speed at ambient temperature.