>ISO Standards>ISO 15309:2013-Implants for surgery — Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices
immediate downloadReleased: 2013
ISO 15309:2013-Implants for surgery — Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

ISO 15309:2013

ISO 15309:2013-Implants for surgery — Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

Format
Availability
Price and currency
English PDF
Immediate download
Printable
82.35 USD
English Hardcopy
In stock
82.35 USD
French PDF
Immediate download
Printable
82.35 USD
French Hardcopy
In stock
82.35 USD
Standard´s number:ISO 15309:2013
Pages:6
Edition:1
Released:2013
DESCRIPTION

ISO 15309:2013


ISO 15309:2013 specifies a method for the thermal analysis of Poly Ether Ether Ketone (PEEK) that is for use in the manufacture of implantable medical devices, using differential scanning calorimetry (DSC). The transition temperatures to be determined are the glass transition temperature (Tg), the melting temperature (Tm) and the crystallization temperature on cooling (Tc).