Homepage>ISO Standards>ISO 22848:2021-Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
download between 0-24 hoursReleased: 2021
ISO 22848:2021-Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

ISO 22848:2021

ISO 22848:2021-Corrosion of metals and alloys — Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

Format
Availability
Price and currency
English PDF
Immediate download
155.00 EUR
English Hardcopy
In stock
155.00 EUR
Standard´s number:ISO 22848:2021
Pages:25
Edition:1
Released:2021
Language:English
DESCRIPTION

ISO 22848:2021


This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave. The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.