ISO 7539-12:2023-Corrosion of metals and alloys — Stress corrosion testing-Part 12: Requirements for atmospheric stress corrosion cracking testing

ISO 7539-12:2023

ISO 7539-12:2023-Corrosion of metals and alloys — Stress corrosion testing-Part 12: Requirements for atmospheric stress corrosion cracking testing

Format
Availability
Price and currency
English PDF
Immediate download
70.00 EUR
English Hardcopy
In stock
70.00 EUR
French PDF
Immediate download
70.00 EUR
French Hardcopy
In stock
70.00 EUR
Standard´s number:ISO 7539-12:2023
Pages:11
Edition:1
Released:2023
DESCRIPTION

ISO 7539-12:2023


This document specifies the general requirements for designing and conducting tests to assess the susceptibility of metals and alloys to stress corrosion cracking under atmospheric exposure conditions. The testing methodology includes exposure to natural environments and environments in artificially accelerated laboratory tests. Applications include aluminium and its alloys in aerospace and construction; stainless steels in construction, pressure vessels, and nuclear waste containment; high strength low alloy steels in automotive, construction, and in lifting chains.